Poly(ɛ-caprolactone) (PCL)
A semi-crystalline polymer with a low melting temperature and high elongation at break.
- Degradation
- 3–4 years
- Elongation
- 300–1000%
Good solubility and a short degradation time: nano- and micro-particulate drug formulations and extended-release coatings.
Statistical copolymers of D,L-lactide with glycolide (PLGA) are characterized by good solubility and a short degradation time.
They are mainly used to create nano- and micro-particulate drug formulations and extended-release coatings. The release kinetics of the active agent can be tuned by changing the composition and molecular weight of the polymer.
| D,L-lactide / glycolide ratio | 85/15, 75/25, 50/50 |
|---|---|
| Degradation time | 1 to 6 months |
| Glass transition temperature | 40–50 °C |
| Young's modulus | 1–2 GPa |
| Tensile strength | 30–40 MPa |
| Elongation at break | 1–10% |
A semi-crystalline polymer with a low melting temperature and high elongation at break.
Higher elongation at break than polylactide and faster degradation; properties are set by the monomer ratio.
A biocompatible thermoplastic aliphatic polyester based on L- or D,L-lactide; feedstock is annually renewable corn and sugar cane.