Poly(L-lactide-co-ɛ-caprolactone) (PLCL)

Higher elongation at break than polylactide and faster degradation; properties are set by the monomer ratio.

Flexible translucent PLCL ribbon loop beside clear pellets.
Flexible translucent PLCL ribbon loop beside clear pellets.
Polymers

Copolymers of L-lactide with ɛ-caprolactone offer higher elongation at break than polylactide and degrade faster.

The degradation time and mechanical properties are set by the L-lactide / ɛ-caprolactone ratio in the copolymer.

Specifications

Specifications: Poly(L-lactide-co-ɛ-caprolactone) (PLCL)
L-lactide / ɛ-caprolactone ratio90/10, 75/25, 50/50
Degradation time3 to 18 months
Glass transition temperature20 to 50 °C
Melting temperature120 to 180 °C
Young's modulus0.3–1.5 GPa
Tensile strength20–50 MPa
Elongation at break30–1000%

Applications

  • Vascular implants
  • Orthopedic trauma devices
  • Aesthetic medicine products
  • Regenerative medicine
Questions and answers

Frequent questions.

Which polymer should I choose for a vascular implant?
Polylactide, PCL and PLCL: fibers and tubes keep their mechanical properties while the vessel recovers, then degrade into safe by-products.
What degradation times do your polymers have?
From 1 month to 5 years depending on the material: PLGA 1–6 months, PGA and PGLA 2–12 months, PLCL 3–18 months, polylactide 6 months to 5 years, PCL 3–4 years. Degradation time is tuned by polymer composition and molecular weight.
Portfolio

Other solutions.

All solutions
Translucent ivory polylactide pellets in a shallow glass dish.
PolymersBioresorbable

Polylactide (PLLA, PDLLA)

A biocompatible thermoplastic aliphatic polyester based on L- or D,L-lactide; feedstock is annually renewable corn and sugar cane.

Degradation
6 months to 5 years
Young's modulus
1.5–4 GPa
Coiled white braided PGA and PGLA suture fibers beside a clear monofilament.
Polymers

Polyglycolide (PGA) and PGLA

High mechanical properties and an adjustable degradation time; the basis of fibers, sutures and surgical devices.

Degradation
2–12 months
Tensile strength
50–100 MPa
Ivory PLGA granules in a sample vial and glass dish.
PolymersPharma

Poly(D,L-lactide-co-glycolide) (PLGA)

Good solubility and a short degradation time: nano- and micro-particulate drug formulations and extended-release coatings.

Degradation
1–6 months
Composition
85/15, 75/25, 50/50