Composition
Monomers define the polymer type and its behavior in the body.
- L-lactide
- DL-lactide
- glycolide
- ɛ-caprolactone
- trimethylene carbonate
Biodegradable medical polymers meet international quality standards for use in medicine and pharma. We help you choose the polymer with the properties your task requires.
Biodegradable polymers are high-molecular-weight compounds used to make temporary implantable medical devices. Once the device has done its job, the material degrades in the body into safe by-products.
Monomers define the polymer type and its behavior in the body.
From 1,000 to 500,000 Da (1–500 kDa). It sets mechanical strength and degradation time: from low-molecular grades for drug formulations to high-molecular grades for implants.
They affect hydrolysis rate and the release kinetics of the active substance.
Generated material studies illustrate product forms; specifications are listed below.
Material images are generated studies. Consult the tables for grade specifications.
We offer a wide range of medical polymers based on cyclic esters, with different compositions, molecular weights (1 to 500 kDa) and end groups. Full specifications of each material (composition, degradation time, temperatures, mechanics and fields of application) are below.
A biodegradable, biocompatible, thermoplastic aliphatic polyester whose monomer is the cyclic dimer of lactic acid (L- or D,L-lactide).
The feedstock for lactic acid production is annually renewable resources such as corn and sugar cane. The properties and supramolecular structure of polylactide vary over a wide range with the content of L- and D-form lactic acid units in the polymer.
Scroll horizontally to explore the chart
| Grade | L units / D units |
|---|---|
| 100/0 | 100/0 |
| 50/50 | 50/50 |
| 70/30 | 70/30 |
| 0/100 | 0/100 |
| L/D unit ratio | 100/0, 50/50, 70/30, 0/100 |
|---|---|
| Degradation time | 6 months to 5 years |
| Glass transition temperature | 45–60 °C |
| Melting temperature | 150–200 °C |
| Young's modulus | 1.5–4 GPa |
| Tensile strength | 40–60 MPa |
| Elongation at break | 1–10% |
Polyglycolide (PGA) and poly(glycolide-co-L-lactide) (PGLA) offer high mechanical properties and an adjustable degradation time.
They are widely used to produce fibers, sutures and various medical devices for surgery.
Scroll horizontally to explore the chart
| Grade | Glycolide / L-lactide |
|---|---|
| 100/0 | 100/0 |
| 90/10 | 90/10 |
| 15/85 | 15/85 |
| Glycolide / L-lactide ratio | 100/0, 90/10, 15/85 |
|---|---|
| Degradation time | 2 to 12 months |
| Glass transition temperature | 35–50 °C |
| Melting temperature | 180–230 °C |
| Young's modulus | 3–7 GPa |
| Tensile strength | 50–100 MPa |
| Elongation at break | 1–10% |
Statistical copolymers of D,L-lactide with glycolide (PLGA) are characterized by good solubility and a short degradation time.
They are mainly used to create nano- and micro-particulate drug formulations and extended-release coatings. The release kinetics of the active agent can be tuned by changing the composition and molecular weight of the polymer.
Scroll horizontally to explore the chart
| Grade | D,L-lactide / Glycolide |
|---|---|
| 85/15 | 85/15 |
| 75/25 | 75/25 |
| 50/50 | 50/50 |
| D,L-lactide / glycolide ratio | 85/15, 75/25, 50/50 |
|---|---|
| Degradation time | 1 to 6 months |
| Glass transition temperature | 40–50 °C |
| Young's modulus | 1–2 GPa |
| Tensile strength | 30–40 MPa |
| Elongation at break | 1–10% |
Poly(ɛ-caprolactone) is a semi-crystalline biodegradable polymer produced by polymerization of ɛ-caprolactone.
It has a low melting temperature and high elongation at break.
Scroll horizontally to explore the chart
| Grade | ɛ-caprolactone / Other units |
|---|---|
| 100/0 | 100/0 |
| Degradation time | 3 to 4 years |
|---|---|
| Glass transition temperature | −60 °C |
| Melting temperature | 60–65 °C |
| Young's modulus | 0.2–0.4 GPa |
| Tensile strength | 20–40 MPa |
| Elongation at break | 300–1000% |
Copolymers of L-lactide with ɛ-caprolactone offer higher elongation at break than polylactide and degrade faster.
The degradation time and mechanical properties are set by the L-lactide / ɛ-caprolactone ratio in the copolymer.
Scroll horizontally to explore the chart
| Grade | L-lactide / ɛ-caprolactone |
|---|---|
| 90/10 | 90/10 |
| 75/25 | 75/25 |
| 50/50 | 50/50 |
| L-lactide / ɛ-caprolactone ratio | 90/10, 75/25, 50/50 |
|---|---|
| Degradation time | 3 to 18 months |
| Glass transition temperature | 20 to 50 °C |
| Melting temperature | 120 to 180 °C |
| Young's modulus | 0.3–1.5 GPa |
| Tensile strength | 20–50 MPa |
| Elongation at break | 30–1000% |
| Parameter | Polylactide | PGA / PGLA | PLGA | PCL | PLCL |
|---|---|---|---|---|---|
| Monomer ratio | L/D 100/0, 50/50, 70/30, 0/100 | glycolide/L-lactide 100/0, 90/10, 15/85 | D,L-lactide/glycolide 85/15, 75/25, 50/50 | — | L-lactide/ɛ-CL 90/10, 75/25, 50/50 |
| Degradation time | 6 months to 5 years | 2–12 months | 1–6 months | 3–4 years | 3–18 months |
| Glass transition temperature | 45–60 °C | 35–50 °C | 40–50 °C | −60 °C | 20–50 °C |
| Melting temperature | 150–200 °C | 180–230 °C | — | 60–65 °C | 120–180 °C |
| Young's modulus | 1.5–4 GPa | 3–7 GPa | 1–2 GPa | 0.2–0.4 GPa | 0.3–1.5 GPa |
| Tensile strength | 40–60 MPa | 50–100 MPa | 30–40 MPa | 20–40 MPa | 20–50 MPa |
| Elongation at break | 1–10% | 1–10% | 1–10% | 300–1000% | 30–1000% |
Scroll horizontally to explore the chart
| Polymer | Range |
|---|---|
| Polylactide | 6 months to 5 years |
| PGA / PGLA | 2 to 12 months |
| PLGA | 1 to 6 months |
| PCL | 3 to 4 years |
| PLCL | 3 to 18 months |
Scroll horizontally to explore the chart
| Polymer | Range |
|---|---|
| Polylactide | 1.5–4 GPa |
| PGA / PGLA | 3–7 GPa |
| PLGA | 1–2 GPa |
| PCL | 0.2–0.4 GPa |
| PLCL | 0.3–1.5 GPa |
No answer here? Write to us and a process engineer will reply on the substance of your task.
Ask a questionTo the customer's specification we can synthesize a polymer with a precisely defined composition, molecular weight, modified end groups, special architecture and more.